Bar, Plât a Thaflen Dur Di-staen 15-5PH
Mar 10, 2026
Gadewch neges



| Safonol |
AMS 5659, AMS 5823, AMS 5862, ASTM A564 / A564M, ASTM A693 |
|---|---|
| Gradd |
0Cr15Ni5Cu4Nb, 1.4545, S15500 |
| Hyd |
1000 mm-6000 mm (39.37-236.22 i mewn), Wedi'i addasu |
| Diamedr |
Bar: 6 mm-300 mm (0.24-12 i mewn), Wedi'i addasu |
| Meddwl |
Wedi'i addasu, Plât: 6 mm-100 mm (0.24-3.94 i mewn), Taflen: 0.5 mm-6 mm (0.02-0.24 i mewn) |
| Lled Llawn |
Wedi'i Addasu, Taflen a Phlât: 1000 mm-2000 mm (39.37-78.74 i mewn) |
| Gorffen Arwyneb |
2B, 2D, BA, Gorchuddio, etc., Ground, Mill, No.1, No.4, Peeled, Polished, Turned |
| Ffurf |
15-5PH Bar wedi'i ffugio, 15- Plât 5PH, Plât sgleinio 15-5PH, dalen 15-5PH, dalen dymheru 15-5PH, Coil, Bar Wedi'i Dynnu'n Oer, Plât Wedi'i Rolio'n Oer, ac ati, Bar Fflat, Dalen wedi'i rolio'n boeth, Bar hirsgwar, Gwialen, Bar Stondin, Bar Sgwâr |
Termau Busnes
| Termau | Manyleb |
|---|---|
| Isafswm Nifer Archeb: | 5 Tunnell |
| Pris: | I'w drafod |
| Manylion Pecynnu: |
Yn ôl y Gofyn |
| Amser Cyflenwi: | O fewn 7-10 Diwrnod Gwaith |
| Telerau Talu: | T/T, L/C, Cerdyn Credyd |
| Gallu Cyflenwi: | 100000 tunnell y mis |
| Ardystiad: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Allforio i: |
Unol Daleithiau, Ffrainc, Japan, yr Almaen, yr Eidal, Sbaen, y Deyrnas Unedig, Taiwan, Twrci, Korea, Brasil, Awstria, yr Iseldiroedd, Mecsico, India, Gwlad Pwyl, Fietnam, Ffederasiwn Rwsia, ac ati. |
Anfon ymchwiliad