Bar Dur Di-staen 15-5PH, Plât a Thaflen ar gyfer cwsmer
Mar 16, 2026
Gadewch neges



| Safonol | AMS 5659, AMS 5823, AMS 5862, ASTM A564 / A564M, ASTM A693 |
|---|---|
| Gradd | 0Cr15Ni5Cu4Nb, 1.4545, S15500 |
| Hyd | 1000 mm-6000 mm (39.37-236.22 i mewn), Wedi'i addasu |
| Diamedr | Bar: 6 mm-300 mm (0.24-12 i mewn), Wedi'i addasu |
| Meddwl | Wedi'i addasu, Plât: 6 mm-100 mm (0.24-3.94 i mewn), Taflen: 0.5 mm-6 mm (0.02-0.24 i mewn) |
| Lled Llawn | Wedi'i Addasu, Taflen a Phlât: 1000 mm-2000 mm (39.37-78.74 i mewn) |
| Gorffen Arwyneb | 2B, 2D, BA, Gorchuddio, etc., Ground, Mill, No.1, No.4, Peeled, Polished, Turned |
| Ffurf | 15-5PH Bar wedi'i ffugio, 15- Plât 5PH, Plât sgleinio 15-5PH, dalen 15-5PH, dalen dymheru 15-5PH, Coil, Bar Wedi'i Dynnu'n Oer, Plât Wedi'i Rolio'n Oer, ac ati, Bar Fflat, Dalen wedi'i rolio'n boeth, Bar hirsgwar, Gwialen, Bar Stondin, Bar Sgwâr |
Cyfansoddiadau Cemegol
| Cromiwm (Cr) | Nicel (Ni) | Copr (Cu) | Manganîs (Mn) | silicon (Si) | carbon (C) | Ffosfforws (P) | sylffwr (S) | Nitrogen (N) |
|---|
| 14.0 – 15.5 | 3.5 – 5.5 | 2.5 – 4.5 | 1.0 uchafswm | 1.0 uchafswm | 0.07 uchafswm | 0.04 uchafswm | 0.03 uchafswm | 0.10 uchafswm |
Priodweddau Mecanyddol
| Priodweddau | Uned Fetrig | Uned Imperial |
|---|
| Cryfder Tynnol | 1000-1170 MPa | 145-170 ksi |
| Cryfder Cynnyrch | ≥ 1000 MPa | ≥ 145 ksi |
| Caledwch Vickers | 360 HV (nodweddiadol) | 360 HV (nodweddiadol) |
| Caledwch Brinell | 350 HB (nodweddiadol) | 350 HB (nodweddiadol) |
| Caledwch Rockwell | 35 HRC (nodweddiadol) | 35 HRC (nodweddiadol) |
| Elongation | ≥ 10% | ≥ 10% |
| Modwlws Elastig | 200 GPa | 29.0 x 10³ ksi |