201 Taflen Dur Di-staen ar gyfer cwsmer

Mar 16, 2026

Gadewch neges

What is 1.4509 Stainless Steel?What is 1.4845 Stainless Steel?410 Stainless Steel Plate | Sheet

Safonol

ASTM A240, EN 10088-2, GB/T 3280

Gradd

1.4372, SUS201, X12CrMnNiN17-7-5, Z12CMN17-07Az

Hyd

2000 mm-6000 mm (78.74-236.22 i mewn), Wedi'i addasu

Lled Llawn

1000 mm-2000 mm (39.37-78.74 i mewn), Wedi'i addasu

Trwch

0.3 mm-6 mm (0.012-0.24 i mewn), Customized

Gorffen Arwyneb

2B, 8K, BA, ac ati, HL, Rhif 1, Rhif 4

Techneg

Wedi'i dynnu'n oer, wedi'i rolio'n oer, wedi'i rolio'n boeth

Ffurf

Coil, Taflen Rolio Oer, Taflenni boglynnog, ac ati, Plât a Thaflen Fflat, Taflen Rolio Poeth, Taflenni Tyllog, Plât, Taflenni caboledig, Llain, Taflenni Gweadog

 

Cyfansoddiadau Cemegol

Elfencarbon (C)Manganîs (Mn)silicon (Si)Ffosfforws (P)sylffwr (S)Cromiwm (Cr)Nicel (Ni)Nitrogen (N)
         
Cyfansoddiad (%)0.15 uchafswm5.5-7.51.0 uchafswm0.06 uchafswm0.03 uchafswm16.0-18.03.5-5.50.25 uchafswm

Priodweddau Mecanyddol

PriodweddauUned FetrigUned Imperial
   
Cryfder Tynnol655 - 860 MPa95 – 125 ks
Cryfder Cynnyrch450 MPa65 ksi
Caledwch Vickers230 – 270 HV230 – 270 HV
Caledwch Brinell200 - 250 HB200 - 250 HB
Caledwch Rockwell50 – 56 HRC50 – 56 HRC
Elongation20%20%
Modwlws Elastig200 GPa29 x 10^6 psi

Anfon ymchwiliad