410 Stainless Steel PipeWhat is 1.4565 Stainless Steel?What is 1.4537 Stainless Steel?

Safonol

ASTM A240, ASTM A276, ASTM A479, ASTM A789, ASTM A790

Gradd

1.4410, S32750, S32760, X2CrNiMoN25-7-4

Hyd

Bar: 3 m-6 m (10-20 tr), wedi'i addasu, pibell: 6 m-12 m (20-40 tr)

Diamedr

Bar: 10 mm-400 mm (0.39-15.75 i mewn), Customized, Pipe (OD): 6 mm-600 mm (0.24-24 i mewn)

Lled Llawn

Coil: 1000 mm-1500 mm (39.37-59.06 i mewn), wedi'i addasu

Trwch

Coil: 0.3 mm-3 mm (0.012-0.12 i mewn), Customized, Pipe (WT): 1 mm-50 mm (0.04-2 i mewn)

Siâp

Wedi'i Addasu, Pibell a Bar: Rownd / Sgwâr / Petryal / Hecsagonol / Fflat

Gorffen Arwyneb

2B, BA, Brwsio, ac ati, Gorffen Drych, Rhif 4, Piclo, Sgleinio, Wedi'i Droi

Ffurf

2507 coil rholio oer, 2507 bar crwn, 2507 pibell di-dor, Coil Annealed, gwialen Bar, ac ati, Ffoil, pibell cyfnewidydd gwres, bar rholio poeth, Plât, Bar sgleinio, gwialen, pibell gron, taflen, stribed, coil stribed, tiwb, pibell wedi'i weldio

 

Cyfansoddiadau Cemegol

ElfenCromiwm (Cr)Nicel (Ni)molybdenwm (Mo)Nitrogen (N)carbon (C)Manganîs (Mn)silicon (Si)Ffosfforws (P)sylffwr (S)
          
Cyfansoddiad (%)24.0 – 26.06.0 – 8.03.0 – 5.00.24 – 0.32≤ 0.03≤ 1.20≤ 0.80≤ 0.035≤ 0.015

Priodweddau Mecanyddol

PriodweddauUned FetrigUned Imperial
   
Cryfder Tynnol800 – 1000 MPa116 - 145 ks
Cryfder Cynnyrch≥ 550 MPa≥ 80 ksi
Caledwch Vickers270 – 310 HV-
Caledwch Brinell260 - 300 HB-
Caledwch Rockwell32 HRC-
Elongation15%15%
Modwlws Elastig200 GPa29.0 × 10^6 psi