304H Taflen Dur Di-staen
Mar 10, 2026
Gadewch neges



| Safonol |
ASME SA240, ASTM A240 / A240M |
|---|---|
| Gradd |
1.4948, S30409, SUS 304H, X7CrNi18-9 |
| Hyd |
2000mm-6000mm (78.7''-236.2''), wedi'i addasu |
| Lled |
1000mm-1500mm (39.4''-59''), Wedi'i addasu |
| Trwch |
0.5mm-100mm (0.02''-3.94''), Wedi'i addasu |
| Gorffen Arwyneb |
2B, 2D, 8K, BA, Brushed, Checkered, Customized, Boglynnog, Ysgythriad, Llinell Gwallt, Drych, Rhif 1, Rhif 4, Rhif 8, Chwyth Tywod |
| Techneg |
Anelio, Plygu, Rholio Oer, Torri, Rholio Poeth |
| Ffurf |
Dalennau wedi'u Brwsio, Taflenni Sioc, Coiliau, Taflenni Rholio Oer, Wedi'u Cymhwyso, Taflenni boglynnog, Dalennau Fflat, Ffoils, Dalennau Galfanedig, Taflenni Rholio Poeth, Taflenni Drych, Taflenni Tyllog, Platiau, Taflenni caboledig, Stribedi |
Termau Busnes
| Termau | Manyleb |
|---|---|
| Isafswm Nifer Archeb: | 5 Tunnell |
| Pris: | I'w drafod |
| Manylion Pecynnu: |
Yn ôl y Gofyn |
| Amser Cyflenwi: | O fewn 7-10 Diwrnod Gwaith |
| Telerau Talu: | T/T, L/C, Cerdyn Credyd |
| Gallu Cyflenwi: | 100000 tunnell y mis |
| Ardystiad: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Allforio i: |
Unol Daleithiau, India, Canada, Chile, y Ffindir, Israel, yr Eidal, Kuwait, Sbaen, y Deyrnas Unedig, ac ati. |
Cyfansoddiad Cemegol
| Elfen | Carbon, C | Cromiwm, Cr | Nicel, Ni | Manganîs, Mn | Silicon, Si | Ffosfforws, P | Sylffwr, S | Nitrogen, N |
|---|
| Cynnwys (%) | 0.04-0.10 | 18.0-20.0 | 8.0-10.5 | Llai na neu'n hafal i 2.00 | Llai na neu'n hafal i 0.75 | Llai na neu'n hafal i 0.045 | Llai na neu'n hafal i 0.030 | Llai na neu'n hafal i 0.10 |
Priodweddau Mecanyddol
| Eiddo | Metrig | Ymerodrol |
|---|
| Cryfder Tynnol | 515-860 MPa | 74-125 ksi |
| Cryfder Cynnyrch | 205-515 MPa | 29.7-74 ksi |
| Caledwch Brinell (HB) | 217-269 | 217-269 |
| Caledwch Rockwell (HRB) | – | – |
| Caledwch Vickers (HV) | – | – |
| Elongation at Break | 40-50% | 40-50% |
| Modwlws Young | 193 GPa | 28 msi |
Anfon ymchwiliad