| Safonol |
ASTM A213, ASTM A269, ASTM A312 |
|---|---|
| Gradd |
1.4307, SUS304L, UNS S30403 |
| Hyd |
Pibell: 6 m - 12 m (20' - 40 '), Tiwbiau: 3m - 6m (10' - 20 '), Wedi'i addasu |
| Diamedr Allanol |
Pibell: 6 mm - 610 mm (0.24'' - 24''), Tiwbiau: 3 mm - 101.6 mm (1/8'' - 4''), Wedi'i addasu |
| Trwch Wal |
Pibell: 0.5 mm - 25 mm (0.02'' - 1''), Tiwbiau: 0.5 mm - 6 mm (0.020'' - 0.236''), Wedi'i addasu |
| Gorffen Arwyneb |
2B, 2D, 8K, BA, Brwsio, Sioc, Wedi'i Addasu, boglynnog, Ysgythriad, Llinell Gwallt, Drych, Rhif 1, Rhif 4, Rhif 8, Chwyth Tywod |
| Techneg |
Anelio, Lluniadu Oer, Rholio Oer, Rholio Poeth, Piclo, Weldio |
| Ffurf |
Tiwbiau Capilari, Pibell / Tiwbiau Coiled, ERW / Pibell SAW, ac ati, Pibell / Tiwbiau Galfanedig, Pibell / Tiwbiau Rolio Poeth / Oer, Crwn / Sgwâr / hirsgwar / hirgrwn / pibell / tiwbiau hecsagonol, tiwbiau misglwyf, pibell / tiwbiau wedi'u weldio / di-dor |
Cyfansoddiad Cemegol
| Elfen | Cromiwm, Cr | Nicel, Ni | Manganîs, Mn | Silicon, Si | Carbon, C | Ffosfforws, P | Sylffwr, S | Nitrogen, N | Haearn, Fe |
|---|
| Cynnwys (%) | 18.0-20.0 | 8.0-12.0 | Llai na neu'n hafal i 2.00 | Llai na neu'n hafal i 0.75 | Llai na neu'n hafal i 0.030 | Llai na neu'n hafal i 0.045 | Llai na neu'n hafal i 0.030 | Llai na neu'n hafal i 0.10 | Cydbwysedd |
Priodweddau Mecanyddol
| Eiddo | Metrig | Ymerodrol |
|---|
| Cryfder Tynnol (0% oer-gweithio) | 564 MPa | 81.8 ksi |
| Cryfder Cynnyrch (0% oer-gweithio) | 210 MPa | 30.5 ksi |
| Caledwch Brinell (HB) | – | – |
| Caledwch Rockwell (HRB) | 82 | 82 |
| Caledwch Vickers (HV) | 159 | 159 |
| Elongation ar Egwyl (Mewn 50mm/2") | 58 % | 58 % |
| Modwlws Young | 193 – 200 GPa | 28.0 – 29.0 Msi |