Mae 309 o ddur di-staen yn ddur di-staen austenitig
Apr 14, 2026
Gadewch neges




Termau Busnes
| Termau | Manyleb |
|---|---|
| Isafswm Nifer Archeb: | 5 Tunnell |
| Pris: | I'w drafod |
| Manylion Pecynnu: |
Yn ôl y Gofyn |
| Amser Cyflenwi: | O fewn 7-10 Diwrnod Gwaith |
| Telerau Talu: | T/T, L/C, Cerdyn Credyd |
| Gallu Cyflenwi: | 100000 tunnell y mis |
| Ardystiad: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Allforio i: |
Unol Daleithiau, y DU, Canada, Awstralia, India, De Affrica, Philippines, Korea, Brasil, Rwsia, Seland Newydd, Twrci, Fietnam, Malaysia, yr Almaen, Indonesia, ac ati. |
Cyfansoddiadau Cemegol
| C | Ni | Si | S | Mn | P | Cr | Mo |
|---|
| 0.20 uchafswm | 12.0 – 15.0 | 0.75 uchafswm | 0.03 uchafswm | 2.00 uchafswm | 0.045 uchafswm | 22.0 – 24.0 | – |
Priodweddau Mecanyddol
| Eiddo | Unedau Imperial | Unedau Metrig |
|---|
| Cryfder Tynnol | 70 – 90 ks | 480 – 620 MPa |
| Cryfder Cynnyrch | 35 – 45 ks | 240 – 310 MPa |
| Caledwch Vickers | 150 - 200 HV | 150 - 200 HV |
| Caledwch Brinell | 140 - 160 HB | 140 - 160 HB |
| Caledwch Rockwell | HRB 80-95 | HRB 80-95 |
| Elongation | 30 – 45% | 30 – 45% |
| Modwlws Elastig | 28 – 30 x 10^6 psi | 190 – 210 GPa |