420 1.4021 X20Cr13 Stainless Steel1.4542, S17400, 630, 17-4PH, Precipitation Hardening Stainless Steel440B vs 440C Martensitic Stainless Steels: Mid-Hardness vs Maximum Wear Resistance

🧪 Cyfansoddiad Cemegol

Cyfansoddiad Cemegol:

Elfen Isafswm % Uchafswm % % nodweddiadol Gofyniad ASTM A276
carbon (C) - 0.080 0.035 Llai na neu'n hafal i 0.08
Cromiwm (Cr) 16.0 18.0 17.2 16.0-18.0
Nicel (Ni) 10.0 14.0 12.0 10.0-14.0
molybdenwm (Mo) 2.0 3.0 2.3 2.0-3.0
Manganîs (Mn) - 2.00 1.35 Llai na neu'n hafal i 2.00
silicon (Si) - 0.75 0.38 Llai na neu'n hafal i 0.75
Ffosfforws (P) - 0.045 0.025 Llai na neu'n hafal i 0.045
sylffwr (S) - 0.030 0.012 Llai na neu'n hafal i 0.030
Nitrogen (N) - 0.10 0.05 Llai na neu'n hafal i 0.10
Haearn (Fe) Cydbwysedd Cydbwysedd 66.1 Cydbwysedd

⚙️ Priodweddau Mecanyddol

Priodweddau Mecanyddol:

Eiddo Gofyniad ASTM Gwerth Nodweddiadol Dull Prawf Tymheredd
Cryfder Tynnol 515 MPa min 620 MPa ASTM A370 Tymheredd yr Ystafell
Cryfder Cnwd (0.2%) 205 MPa min 310 MPa ASTM A370 Tymheredd yr Ystafell
Elongation 30% mun 40% ASTM A370 Tymheredd yr Ystafell
Caledwch (Brinell) 217 HB uchafswm 185 HB ASTM E10 Tymheredd yr Ystafell
Caledwch (Rockwell B) 95 HRB ar y mwyaf 88 HRB ASTM E18 Tymheredd yr Ystafell
Modwlws Elastigedd - 200 GPa ASTM E111 Tymheredd yr Ystafell
Effaith Egni (Charpy V) - 325+ J ASTM E23 Tymheredd yr Ystafell