420 Cynhyrchion Dur Di-staen

Mar 23, 2026

Gadewch neges

304 Stainless Steel Coil for Deep Drawing and Stamping304L Stainless Steel Pipe for Chemical Fluid Transportation304 Stainless Steel Sheet for Architectural Decoration

 

Cyfansoddiadau Cemegol

Elfen

C (Carbon)

Cr (Cromiwm)

Mn (Manganîs)

Si (Silicon)

P (ffosfforws)

S (Sylffwr)

Ni (nicel)

Haearn (Fe)

Haearn (Fe)

Cynnwys 0.15% – 0.40% 12.0% – 14.0% 1.0% ar y mwyaf 1.0% ar y mwyaf 0.04% ar y mwyaf 0.03% ar y mwyaf 0.75% ar y mwyaf Cydbwysedd \

Priodweddau Mecanyddol

Priodweddau

Uned Fetrig

Uned Imperial

Cryfder Tynnol 655 - 860 MPa 95 – 125 ks
Cryfder Cynnyrch 450 MPa 65 ksi
Caledwch Vickers 230 – 270 HV 230 – 270 HV
Caledwch Brinell 200 - 250 HB 200 - 250 HB
Caledwch Rockwell 50 – 56 HRC 50 – 56 HRC
Elongation 20% 20%
Modwlws Elastig 200 GPa 29 x 10^6 psi

Anfon ymchwiliad