Pibell Dur Di-staen Super Austenitig 904L ar gyfer Gwasanaeth Cyrydol
Mar 16, 2026
Gadewch neges



| Safonol |
ASTM A269, ASTM A312, EN 10216-5, ISO 1127 |
|---|---|
| Gradd |
1.4539, 904S13, N08904, X1NiCrMoCu25-20-5 |
| Hyd |
6 m-12 m (20-40 tr), Wedi'i addasu |
| 0D |
6 mm-2000 mm (0.24-78.74 i mewn), Customized |
| WT |
0.5 mm-30 mm (0.02-1.18 i mewn), Wedi'i addasu |
| Gorffen Arwyneb |
2B, 8K, BA, Brwsio, Customized, Rhif 4, Wedi'u Peeled, Wedi'u sgleinio |
| Siâp |
Wedi'i Addasu, Fflat, Hecsagonol, Hydrolig, Hirgrwn, Petryal, Crwn, Sgwâr |
| Ffurf |
Pibell a Thiwb 904L, Pibell Ddi-dor 904L, Pibell Wedi'i Weldio 904L, Tiwbiau wedi'u Torchi, Pibell ERW, Tiwbiau Glanweithdra a Siapiau wedi'u Cymhwyso., Pibell Wedi'i Weldio Troellog, Pibell Sgwâr a Phetryal, U{4}}Tiwbiau Plygu |
Termau Busnes
| Termau | Manyleb |
|---|---|
| Isafswm Nifer Archeb: | 5 Tunnell |
| Pris: | I'w drafod |
| Manylion Pecynnu: |
Yn ôl y Gofyn |
| Amser Cyflenwi: | O fewn 7-10 Diwrnod Gwaith |
| Telerau Talu: | T/T, L/C, Cerdyn Credyd |
| Gallu Cyflenwi: | 100000 tunnell y mis |
| Ardystiad: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Allforio i: |
Unol Daleithiau, Awstralia, Brasil, Canada, y Ffindir, India, yr Eidal, Corea, yr Iseldiroedd, Gwlad Pwyl, Ffederasiwn Rwsia, Sweden, y Deyrnas Unedig, Hongkong, Singapore, y Swistir, yr Almaen, Ffrainc, Indonesia, Iran, ac ati. |
Cyfansoddiadau Cemegol
| Elfen | Cromiwm (Cr) | Nicel (Ni) | molybdenwm (Mo) | Copr (Cu) | carbon (C) | Manganîs (Mn) | silicon (Si) | Ffosfforws (P) | sylffwr (S) |
|---|
| Cynnwys (%) | 19.0-23.0 | 23.0-28.0 | 4.0-5.0 | 1.0-2.0 | Llai na neu'n hafal i 0.020 | Llai na neu'n hafal i 2.00 | Llai na neu'n hafal i 1.00 | Llai na neu'n hafal i 0.045 | Llai na neu'n hafal i 0.035 |