Dur Di-staen Martensitig Caledadwy: Gradd 410 / 1.4006
Apr 09, 2026
Gadewch neges




Cyfansoddiad Cemegol
| 1.4006 Dur | EN 10088-3:2005 |
|---|---|
| Elfen gemegol | % Presennol |
| carbon (C) | 0.08 - 0.15 |
| Cromiwm (Cr) | 11.50 - 13.50 |
| silicon (Si) | 0.0 - 1.00 |
| Manganîs (Mn) | 0.0 - 1.50 |
| ffosfforws (P) | 0.0 - 0.04 |
| sylffwr (S) | 0.0 - 0.02 |
| Nicel (Ni) | 0.0 - 0.75 |
| Haearn (Fe) | Cydbwysedd |
Priodweddau
| Eiddo Corfforol | Gwerth |
|---|---|
| Dwysedd | 7.75 g / cm³ |
| Ehangu Thermol | 9.9 x 10-6/K |
| Modwlws Elastigedd | 300 GPa |
| Dargludedd Thermol | 24.9 W/m.K |
| Gwrthiant Trydanol | 0.57 x 10-6 Ω.m |
| Bar - Hyd at 160mm Dia neu Drwch | EN 10088-3:2005 |
|---|---|
| Eiddo Mecanyddol | Gwerth |
| Straen Prawf | 450 Min MPa |
| Cryfder Tynnol | 650 - 850 MPa |
| Elongation A | 15 Munud % |