SS 420 Taflenni Gradd / platiau / coiliau
Mar 10, 2026
Gadewch neges



|
Graddau dur |
AISI420 (1.4016) |
|
Cynhyrchu |
Oer{0}}wedi'i rolio |
|
Safonol |
ASTM A240/A480 |
|
Trwch |
Isafswm: 0.4mm Uchafswm: 6.0mm |
|
Lled |
1000mm, 1250mm, 1500mm, 2000mm, meintiau eraill ar gais |
|
Gorffen |
2B, BA, MATT, M.PVC, N4, N5, SB, HR, N8, Sail olew wedi'i sgleinio'n wlyb, Mae'r ddwy ochr wedi'i sgleinio ar gael |
|
Gorchuddio |
Gorchudd PVC arferol / laser |
|
Pwysau pecyn |
1.0-2.2 tunnell |
|
Cais |
Offer meddygol, Diwydiant bwyd, Deunydd adeiladu, Offer cegin, gril barbeciw, Adeiladu adeiladau, Offer trydan, |
Dur Di-staen 420 Meintiau Coil
|
Graddau dur |
AISI420 (1.4016) |
|
Cynhyrchu |
Oer{0}}rholio, poeth-rholio |
|
Safonol |
ASTM A240/A480 |
|
Trwch |
Isafswm: 0.4mm Uchafswm: 10.0mm |
|
Lled |
1000mm, 1250mm, 1500mm, 2000mm, meintiau eraill ar gais |
|
Gorffen |
1D, 2B, BA, N4, N5, SB, HL, N8, sylfaen olew wedi'i sgleinio'n wlyb, y ddwy ochr wedi'i sgleinio ar gael |
|
Gorchuddio |
Gorchudd PVC arferol / laser |
|
Pwysau pecyn |
1.0-10.0 tunnell |
|
Pwysau pecyn |
Trwch 3-6mm: 2.0-10.0 tunnell |
|
Cais |
Offer meddygol, Diwydiant bwyd, Deunydd adeiladu, Offer cegin, gril barbeciw, Adeiladu adeiladau, Offer trydan, |
Dur Di-staen 420 Meintiau Platiau
Graddau dur |
AISI420 (1.4016) |
|
Cynhyrchu |
Hot{0}}rholio |
|
Safonol |
ASTM A240/A480 |
|
Trwch |
Safon: 3.0mm-30.0mm |
|
Lled |
1000mm, 1250mm, 1500mm, 2000mm, meintiau eraill ar gais |
|
Pwysau pecyn |
1.0-4.0 tunnell |
|
Cais |
Offer meddygol, Diwydiant bwyd, Deunydd adeiladu, Offer cegin, gril barbeciw, Adeiladu adeiladau, Offer trydan, |