Dur Di-staen Gradd 420J2 - Gradd Offeryn Caledwch Uchel

Feb 05, 2026

Gadewch neges

Stainless Steel Grade 304 - Food Grade & Corrosion ResistantStainless Steel Grade 321 - High Temperature Resistant GradeSUS316Ti Stainless Steel Plate & Coil: Titanium-Stabilized High-Temp Welding Plate/Coil

Safonau a Graddau Cyfwerth

 

UNS EN ASTM DIN GOST GB

SUS420J2

1.4034

Math 420 (Uchel-C)

X46Cr13

40Х13

4Cr13

 

 

Cyfansoddiad Cemegol

 

Gradd Safonol C Cr Ni Mn Si P S Fe

420J2

JIS G 4303

0.26–0.40

12.0–14.0

Llai na neu'n hafal i 1.0

Llai na neu'n hafal i 1.0

Llai na neu'n hafal i 1.0

Llai na neu'n hafal i 0.04

Llai na neu'n hafal i 0.03

Cydbwysedd

1.4034

EN 10088-2

0.43–0.50

12.5–14.5

Llai na neu'n hafal i 1.0

Llai na neu'n hafal i 1.0

Llai na neu'n hafal i 1.0

Llai na neu'n hafal i 0.04

Llai na neu'n hafal i 0.03

Cydbwysedd

4Cr13

GB/T 1220

0.36–0.45

12.5–14.5

-

-

Llai na neu'n hafal i 1.0

Llai na neu'n hafal i 0.04

Llai na neu'n hafal i 0.03

Cydbwysedd

 

 

Priodweddau Mecanyddol o 420J2

 

Gradd Safonol Cryfder Tynnol Cryfder Cynnyrch Elongation Caledwch (Brinell)

SUS420J2

JIS G 4303

Yn fwy na neu'n hafal i 740 MPa

Yn fwy na neu'n hafal i 300 MPa

Yn fwy na neu'n hafal i 15 %

Llai na neu'n hafal i 217 HBW (annealed)

1.4034

EN 10088-2

Yn fwy na neu'n hafal i 750 MPa

Yn fwy na neu'n hafal i 300 MPa

Yn fwy na neu'n hafal i 12 %

Llai na neu'n hafal i 217 HBW

4Cr13

GB/T 1220

Yn fwy na neu'n hafal i 750 MPa

Yn fwy na neu'n hafal i 300 MPa

Yn fwy na neu'n hafal i 12 %

Llai na neu'n hafal i 217 HBW