SUS347 Dur Di-staen: Niobium-Nodweddion Aloi Sefydlog

Jan 06, 2026

Gadewch neges

316Ti vs 316L Austenitic Stainless Steels: Stabilized High-Temp vs Low-Carbon WeldableSUS310S Stainless Steel: High-Temperature Corrosion ResistanceSUS316 vs SUS316L: Core Differences in Corrosion Resistance

347 o Raddau Cyfatebol

 

ASTM JIS UNS EN DIN GOST GB

347

SUS347

S34700

1.4550

X6CrNiNb18-10

08Х18Н12Б

06Cr18Ni11Nb

 

 

Cyfansoddiad Cemegol

 

Gradd Safonol C (%) Cr (%) Ni (%) Nb+Ta (%) Mn (%) Si (%) P (%) S (%) Fe (%)

347

ASTM A240

Llai na neu'n hafal i 0.08

17.0–19.0

9.0–13.0

10×C–1.0

Llai na neu'n hafal i 2.0

Llai na neu'n hafal i 1.0

Llai na neu'n hafal i 0.045

Llai na neu'n hafal i 0.03

Cydbwysedd

1.4550

EN 10088-2

Llai na neu'n hafal i 0.08

17.0–19.0

9.0–13.0

8×C–1.0

Llai na neu'n hafal i 2.0

Llai na neu'n hafal i 1.0

Llai na neu'n hafal i 0.045

Llai na neu'n hafal i 0.03

Cydbwysedd

SUS347

JIS G 4304
JIS G 4305

Llai na neu'n hafal i 0.08

17.0–19.0

9.0–13.0

8×C–1.0

Llai na neu'n hafal i 2.0

Llai na neu'n hafal i 1.0

Llai na neu'n hafal i 0.045

Llai na neu'n hafal i 0.03

Cydbwysedd

 

 

Mae 347 o ddur di-staen yn darparu ymwrthedd ardderchog i ocsidiad a graddio ar dymheredd uchel, sy'n debyg i 321 ac yn well na 304 mewn gwresogi cylchol.

Mae'r ychwanegiad niobium yn cynnig amddiffyniad rhag cyrydiad rhyng-gronynnog, yn enwedig ar ôl weldio neu amlygiad i 425-850 gradd. Fodd bynnag, ar gyfer gwasanaeth tymheredd uchel parhaus (dros 600 gradd ), argymhellir 347H oherwydd ei gryfder ymgripiad uwch o gynnwys carbon uwch.