904 l graddau dur gwrthstaen: 00 cr20ni25mo4. 5 cu/UNS: N08904 / EN: 1.4539
Amrediadau cyfansoddiad o ddur di-staen gradd 904L
|
Gradd |
C |
Mn |
Si |
P |
S |
Cr |
Mo |
Ni |
Cu |
|
|
904L |
min. max. |
- 0.02 |
- 2 |
- 1 |
- 0.045 |
- 0.035 |
19 23 |
4 5 |
23 28 |
1 2 |
Priodweddau mecanyddol dur gwrthstaen gradd 904L
|
Gradd |
Cryfder Tynnol (MPa) min |
Cryfder Cynnyrch 0.2% Prawf (MPa) min |
Elongation (% mewn 50mm) min |
Caledwch |
|
|
Rockwell B (HR B) |
Brinell (HB) |
||||
|
904L |
490 |
220 |
36 |
70-90 nodweddiadol |
150 |