En 10217-7 pibellau diwydiannol dur gwrthstaen
May 07, 2025
Gadewch neges
Nodweddion allweddol en 10217-7 tiwbiau wedi'u weldio
✅ Safonol: En 10217-7
✅ Graddau Deunyddiol: Mae'r graddau cyffredin yn cynnwys 1.4301 (304), 1.4307 (304L), 1.4404 (316L), 1.4435, ac ati.
✅ Math o diwb: Wedi'i weldio (wedi'i weldio yn hydredol)
✅ Ffurfiwyd: Tiwbiau crwn
✅ Gorffeniad arwyneb: Gorffeniad melin, piclo, neu sgleinio (ee, 180 graean, 240 graean, 320 graean)
✅ Ystod diamedr allanol: 13.5 mm i 323.9 mm
✅ Trwch wal: O 1.2 mm hyd at 8.8 mm

En 10217-7 Dimensiynau tiwb dur gwrthstaen (OD × Trwch Wal)
| Diamedr y tu allan (mm) | 1.20 | 1.60 | 2.00 | 2.30 | 2.60 | 2.90 | 3.20 | 3.60 | 4.00 | 4.50 | 5.00 | 5.60 | 6.30 | 7.10 | 8.00 | 8.80 |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 13.50 | ✔ | |||||||||||||||
| 17.20 | ✔ | ✔ | ||||||||||||||
| 21.30 | ✔ | ✔ | ✔ | |||||||||||||
| 26.90 | ✔ | ✔ | ✔ | ✔ | ||||||||||||
| 33.70 | ✔ | ✔ | ✔ | ✔ | ✔ | |||||||||||
| 42.40 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ||||||||||
| 48.30 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | |||||||||
| 60.30 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ||||||||
| 76.10 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ||||||||
| 88.90 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ||||||||
| 101.60 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ||||||||
| 114.30 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ||||||||
| 139.70 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ||||||||
| 168.30 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ||||||||
| 219.10 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ||||||||
| 273.00 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ||||||||
| 323.90 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ |
✅ Chwedl: ✔ yn nodi argaeledd ar gyfer trwch OD a wal penodol.