🧪 Cyfansoddiad Cemegol
| Elfen | Cyfansoddiad (%) |
|---|---|
| carbon (C) | 0.04 - 0.10 |
| Manganîs (Mn) | Llai na neu'n hafal i 2.00 |
| silicon (Si) | Llai na neu'n hafal i 0.75 |
| Ffosfforws (P) | Llai na neu'n hafal i 0.045 |
| sylffwr (S) | Llai na neu'n hafal i 0.030 |
| Cromiwm (Cr) | 17.0 - 20.0 |
| Nicel (Ni) | 9.0 - 13.0 |
| Titaniwm (Ti) | 4×(C+N) mun, 0.70 max |
| Nitrogen (N) | Llai na neu'n hafal i 0.10 |
| Haearn (Fe) | Cydbwysedd |
⚙️ Priodweddau Mecanyddol
| Eiddo | Gwerth |
|---|---|
| Cryfder Tynnol (Tymheredd Ystafell) | Yn fwy na neu'n hafal i 515 MPa |
| Cryfder Cynnyrch (Gwrthbwyso 0.2%) | Yn fwy na neu'n hafal i 205 MPa |
| Elongation (mesurydd 50mm) | Mwy na neu'n hafal i 40% |
| Lleihau Ardal | Yn fwy na neu'n hafal i 50% |
| Caledwch (Brinell) | Llai na neu'n hafal i 217 HB |
| Impact Energy (Charpy V-rhif, Tymheredd yr Ystafell) | Mwy na neu'n hafal i 68 J |
| Modwlws Young | 200 GPa |
| Cryfder Crip (100,000h ar 650 gradd) | 35 MPa |
| Terfyn Blinder (107beiciau) | 240 MPa |
🔬 Priodweddau Corfforol
| Eiddo | Gwerth |
|---|---|
| Dwysedd | 7.90 g / cm³ |
| Ymdoddbwynt | 1400-1450 gradd |
| Dargludedd Thermol (20 gradd) | 16.3 W/m·K |
| Dargludedd Thermol ( 100 gradd ) | 17.8 W/m·K |
| Ehangu Thermol (20-100 gradd) | 17.2×10-6/K |
| Ehangu Thermol (20-500 gradd) | 18.4×10-6/K |
| Cynhwysedd Gwres Penodol | 500 J/kg·K |
| Gwrthiant Trydanol ( 20 gradd ) | 0.72 µΩ·m |
| Athreiddedd Magnetig | 1.02 µr (An-magnetig) |
| Tymheredd Curie | An-magnetig |
📏 Manylebau Cynnyrch
| Manyleb | Opsiynau sydd ar Gael |
|---|---|
| Ffurflenni Cynnyrch | Bariau, Gwialenni, Platiau, Taflenni, Tiwbiau, Pibellau, Gofaniadau, Castings |
| Ystod Diamedr Bar | 6mm - 300mm |
| Ystod Trwch Plât | 3mm - 150mm |
| Ystod Trwch Taflen | 0.5mm - 6mm |
| Diamedr Allanol Tiwb | 6mm - 219mm |
| Cydymffurfiaeth Safonau | ASTM A240, A479, A312, EN 10088-2, JIS G4304, GB/T 1220 |
| Gorffeniadau Arwyneb | Rholio Poeth, Rholio Oer, 2B, BA, Rhif 4, HL, Drych |
| Goddefgarwch Dimensiynol | ±0.1mm i ±0.5mm (yn dibynnu ar ffurf a maint) |
| Dewisiadau Hyd | Hyd safonol neu dorri i fanylebau cwsmeriaid |