🧪 Cyfansoddiad Cemegol
| Elfen | Cyfansoddiad (%) |
|---|---|
| carbon (C) | ≤ 0.08 |
| Manganîs (Mn) | ≤ 2.00 |
| silicon (Si) | ≤ 1.50 |
| Ffosfforws (P) | ≤ 0.045 |
| sylffwr (S) | ≤ 0.030 |
| Cromiwm (Cr) | 24.0 - 26.0 |
| Nicel (Ni) | 19.0 - 22.0 |
| Nitrogen (N) | ≤ 0.10 |
| Haearn (Fe) | Cydbwysedd |
⚙️ Priodweddau Mecanyddol
| Eiddo | Gwerth |
|---|---|
| Cryfder Tynnol (Tymheredd Ystafell) | ≥ 515 MPa |
| Cryfder Cynnyrch (Gwrthbwyso 0.2%) | ≥ 205 MPa |
| Elongation (mesurydd 50mm) | ≥ 40% |
| Caledwch (Brinell) | ≤ 217 HB |
| Caledwch (Rockwell B) | ≤ 95 HRB |
| Impact Energy (Charpy V-rhif) | ≥ 120 J |
| Modwlws Young | 200 GPa |
| Terfyn Blinder (107beiciau) | 240 MPa |
🔬 Priodweddau Corfforol
| Eiddo | Gwerth |
|---|---|
| Dwysedd | 7.98 g / cm³ |
| Ymdoddbwynt | 1400-1450°C |
| Dargludedd Thermol (20°C) | 14.2 W/m·K |
| Cyfernod Ehangu Thermol (20-100°C) | 14.4×10-6/K |
| Cyfernod Ehangu Thermol (20-1000 ° C) | 18.0×10-6/K |
| Cynhwysedd Gwres Penodol | 500 J/kg·K |
| Gwrthiant Trydanol (20°C) | 0.78 µΩ·m |
| Athreiddedd Magnetig | 1.02 µH/m (An-magnetig) |
| Cymhareb Poisson | 0.27-0.30 |
📏 Manylebau Cynnyrch
| Manyleb | Opsiynau sydd ar Gael |
|---|---|
| Ffurflenni Cynnyrch | Bariau crwn, bariau sgwâr, bariau gwastad, cynfasau, platiau, tiwbiau, pibellau, gofaniadau |
| Diamedr Bar Crwn | 6mm - 300mm |
| Trwch Dalen/Plât | 0.5mm - 100mm |
| Diamedr Allanol Tiwb | 6mm - 219mm |
| Cydymffurfiaeth Safonau | ASTM A240, A276, A312, A479, EN 10088-2, JIS G4303, GB/T 1220 |
| Gorffeniadau Arwyneb | Wedi'i rolio'n boeth, wedi'i rolio'n oer, wedi'i anelio'n llachar, wedi'i biclo, wedi'i sgleinio (2B, BA, Rhif 4, Rhif 8) |
| Goddefiad Hyd | ±5mm neu fel y nodir |
| Goddefiant Diamedr | h9, h11, neu fel y pennir |
| Cyflwr | Ateb wedi'i anelio (1050-1100 ° C), wedi'i ddiraddio, wedi'i biclo |